Installation of soft shingle roofing: a full breakdown of the assembly, layers and details
Installing a soft shingle roof is a multi-layer structure (roof assembly) including rafters, vapour barrier, insulation, waterproofing, counter-battens, a continuous base of OSB or plywood, underlay and valley lining, and the final covering of shingle tabs. Each layer performs its own function and is installed in a strict sequence.
What soft (flexible) shingles are and how they are constructed
Soft shingle roofing is a frequent question, so let us look at it in detail. Soft (flexible) shingles are a modern roofing material based on bitumen and glass fibre mat. Let us look at what it consists of, what its features are and how it differs from other coverings.
What flexible shingles are and what they consist of
Flexible shingles are a piece roofing material in the form of flat sheets (shingles) with shaped cut-outs, made from glass fibre mat impregnated with bitumen, with a mineral topping on top and a self-adhesive layer underneath. Each shingle is a multilayer “build-up”: basalt granules protect against ultraviolet radiation, beneath them is a layer of oxidised bitumen with SBS or APP modifiers giving elasticity down to −30 °C, and the glass fibre mat core provides tensile strength of 600–800 N/5 cm in brands such as CertainTeed, IKO and Tegola. The underside is coated with self-adhesive bitumen with a siliconeised film — this is removed before installation, laying the shingles from eaves to ridge with a 15–20 cm overlap. In a sharply continental climate with swings of 20–25 °C per day, it is the multilayer structure that prevents cracking: single-layer cheap equivalents lose elasticity after 3–4 seasons, and cracks appear at the joints, leading to leaks — so for Almaty houses it is better to choose two-layer collections.
Why “soft”: the material's characteristics and advantages
The material is called “soft” because of its ability to bend and take the shape of the base — this allows covering roofs of any complexity, including domes and towers, without trimming. The shingles are installed from eaves to ridge, and each subsequent row overlaps the joints of the previous one, creating a seamless waterproof carpet — unlike metal tiles with their rigid sheet geometry, no drumming noise is heard on a bitumen roof in the rain. The weight of a square metre of flexible shingles is 8–12 kg, which is 4–5 times lighter than ceramic, so the rafter system does not need reinforcing, and the service life of a quality covering reaches 25–50 years with Tegola, Katepal and Shinglas. But only with correct installation of the roof build-up — saving on the underlayment or OSB board reduces the lifespan by 2–3 times, and after 5–7 years bulges appear at the joints, requiring a complete rebuild of the problem area rather than a local repair.
Minimum roof slope for flexible shingles
The minimum slope for flexible shingles is 12° (22%); at a lower slope, water stagnates at the joints of the shingles and penetrates under the covering — on flat roofs at 5–11°, roll-applied bituminous membranes or PVC membranes are used. On shallow slopes of 12–20°, manufacturers Tegola, Katepal and Shinglas require a continuous underlay over the entire area, not only along the eaves, ridge and valleys — this is a mandatory condition of the warranty, not a recommendation. In areas with high snow load of 200–250 kg/m² on slopes of 12–15°, the underlay is additionally secured with roofing nails at a spacing of 20 cm, because the self-adhesive layer can peel off in strong wind. On steep slopes from 30°, an underlay is sufficient only in problem areas, but shingle consumption increases by 10–15% per linear metre of ridge due to the increased overlap — this is important to consider when calculating the budget for a roof of complex shape, especially on houses with an attic.
Comparison of flexible shingles with other roofing materials
| Parameter | Soft tiles | Metal roof tiles | Ondulin | Ceramic tiles |
|---|---|---|---|---|
| Noise from rain | Low | High | Average | Low |
| Installation complexity | Medium | Medium | Low | High |
| Service life | 25–50 years | 20–40 years | 10–15 years | 50–100 years |
| Minimum slope | 12° | 14° | 12° | 22° |
| Suitable for complex roofs | Yes | No (a lot of waste) | Yes | No (heavy) |
| Weight of 1 m² | 8–12 kg | 4–6 kg | 3–4 kg | 40–60 kg |
| Repairability | High (shingle replacement) | Average (sheet replacement) | High (patch repair) | Low (tile replacement) |
On complex roofs with many valleys and abutments, flexible shingles produce 5–10% of waste versus 15–20% for metal roof tiles — the difference directly affects the final cost of the covering, so on houses with broken roof geometry, bituminous shingles prove more cost-effective even at a higher material price per square metre.
Soft roofing build-up — layers from bottom to top
Installing a soft roof is a common question, so let us examine it in detail. The roof assembly is not just a set of layers, but an engineered system where each element performs its own function. Let us look at the correct sequence from bottom to top.
The rafter system is the basis of the roofing assembly
The rafter system is the load-bearing frame of the roof, which bears the weight of all layers of the roof assembly, snow and wind loads; the rafter spacing is usually 600–900 mm. For private houses in Almaty with moderate snow load, boards with a section of 50×150 or 50×200 mm are used — this is sufficient for spans of up to 5–6 metres. With a spacing of 600 mm, the rafters experience less bending than with 900 mm, which allows savings on the cross-section of the timber. If the spacing exceeds 900 mm, additional posts or tie beams are required, otherwise the deflection under snow in winter will exceed permissible norms. The rafter spacing directly affects the thickness of the OSB or plywood: with a spacing of 600 mm, 9 mm is sufficient; with 900 mm — 12 mm is already needed, otherwise the base will flex.
Vapour barrier — protecting the insulation from the inside
The vapour barrier film is laid on the interior side beneath the insulation and protects it from moist air rising from living rooms. In Almaty houses with attics, humidity in winter reaches 50–60 %%, and without a vapour barrier, water vapour condenses inside the mineral wool, sharply reducing its thermal resistance. We use three-layer reinforced polypropylene membranes — they are stronger than single-layer ones and do not tear when fastened with staples. The sheets are laid with an overlap of 15–20 cm, sealing the joints with butyl rubber tape. Choosing the wrong side to lay is one of the most common mistakes: the rough side must face the insulation, the smooth side towards the room, otherwise condensation remains inside.
Insulation — which to choose and what thickness
For soft roofing, mineral or stone wool with a density of 30–50 kg/m³ is used, less often PIR boards; the insulation thickness is calculated according to the climate zone and is usually 200–250 mm. For Almaty, where the design winter temperature reaches –25 °C, the thermal resistance of the roof (R) must be at least 4,5 m²·°C/W — this is provided by 200 mm mineral wool in two layers with overlapping joints. PIR boards at the same thickness give an R of about 5,0, but cost 2–2,5 times more and require cutting to size. Two layers of insulation are mandatory: the first between the rafters, the second below, under or over the rafters, to bridge the cold bridges through the timber. When laying insulation between the rafters it is important that the boards fit tightly — without gaps, otherwise up to 30 % of heat escapes through the gaps and cold bridges form.
Waterproofing (diffusion membrane) — protection from external moisture
The diffusion membrane is laid over the insulation and protects it from moisture that can penetrate through damaged covering or condensation from the inner side of the shingles. In Kazakhstani conditions, where summer rains can be prolonged and snow melts unevenly, the membrane is a mandatory element, not an option. We install only three-layer vapour-permeable membranes with an SD value of less than 0,02 m — they let vapour out of the insulation but do not let water in. The sheets are fixed with a sag of 10–20 mm between the rafters so that condensation flows down rather than being retained. Unlike ordinary waterproofing, a diffusion membrane lets vapour out of the insulation — this is critical, otherwise moisture remains inside and reduces thermal insulation.
Counter-batten and ventilation gap
The counter-batten made of 50×50 mm timber is installed over the waterproofing along the rafters and creates a 50 mm ventilation gap between the membrane and the continuous deck. In Almaty houses, where spring temperature swings reach 15–20 °C per day, this gap acts as a dehumidifier — the airflow draws out condensation, preventing it from accumulating on the OSB. The timber is fixed to each rafter with galvanised nails or screws at least 100 mm long — fixing pitch 400–500 mm. If the gap is made smaller than 50 mm, the airflow rate drops and moisture cannot evaporate in time. Without a counter-batten the waterproofing lies tight against the OSB — condensation does not evaporate, the timber begins to rot, and the roof's service life is reduced to 5–7 years.
Continuous substrate and final covering
A continuous base of OSB-3 or FSF plywood 9–12 mm thick is installed over the counter-battens, and on top of it the underlay and flexible shingle tabs are laid. OSB-3 — is the most common option in Almaty: it is cheaper than plywood (approximately 4500–5500 KZT per sheet of 1250×2500 mm versus 7000–9000 for plywood) and withstands humidity of up to 85 %% without delamination. The boards are laid with their long side across the rafters with staggered offset seams — this distributes the load evenly. A gap of 3–5 mm must be left between OSB boards for thermal expansion — if laid tightly, the boards will buckle in summer and the roof will become wavy.
What substrate is needed under soft tiles
The base for flexible shingles must be even, rigid and moisture-resistant. Let us look at what it is made of, what thickness is used, and how the rafter spacing relates to the choice of boards.
OSB or plywood under soft tiles — which is better
For the base under flexible shingles, OSB-3 (moisture-resistant) or FSF plywood is used — both materials are suitable, but OSB is cheaper and plywood is stiffer at the same thickness. OSB-3 — is an oriented strand board with polymer impregnation, resistant to short-term wetting in rain or snow. FSF plywood is glued with phenol-formaldehyde adhesive, which is not afraid of temperature changes, and thanks to the cross-grained veneer it deflects less over spans between rafters. The price difference is 15-20% in favour of OSB, but on complex roofs (with dormer windows, valleys) plywood is more convenient to cut: it can be cut in any direction without loss of strength. OSB-3 is preferable on roofs with high humidity (for example, near the sea) — it delaminates less when wet than FSF plywood, which can bubble at the edges after several freeze-thaw cycles.
Thickness of OSB and plywood depending on the rafter spacing
| Rafter spacing, mm | OSB-3 thickness, mm | FSF plywood thickness, mm | Note |
|---|---|---|---|
| 600 | 9 | 9 | Minimum thickness for residential buildings |
| 700 | 10 | 10 | Optimal option |
| 800 | 11 | 11 | Counter-batten reinforcement required |
| 900 | 12 | 12 | Maximum spacing for 12 mm |
| 1000 | 15 | 15 | Wide spacing — better to reduce |
The greater the distance between the rafters, the thicker the board must be so as not to deflect under snow load. With a spacing of more than 900 mm, even 12 mm OSB may not hold — in such cases either the spacing is reduced or 15-18 mm is used.
OSB and plywood grade — which to choose
For the base under flexible shingles only OSB-3 (moisture-resistant) or FSF plywood is suitable — OSB-2 and FK plywood are not designed for outdoor conditions and break down quickly. OSB-3 differs from OSB-2 in its moisture-resistant resin content: OSB-2 swells within 2-3 hours when wet, while OSB-3 withstands up to 48 hours without losing its shape. FSF plywood, unlike FK plywood, is glued with phenol-formaldehyde adhesive, which does not delaminate on contact with condensation from the attic side. On the Kazakhstani market OSB-3 is represented by brands such as Egger and Kronospan, and FSF plywood by SVEZA and Chinese equivalents marked FSF. When buying OSB, pay attention to the emission class: E1 — is safe for residential premises, E2 — only for non-residential attics, as it releases more formaldehyde when heated.
How to install a solid substrate correctly
OSB or plywood boards are installed in a staggered pattern (with offset seams) with a gap of 3-5 mm between them and fastened to the counter-battens with screws or twisted nails at a spacing of 150-200 mm. The gap is needed because OSB and plywood expand when heated by the sun by up to 1-2 mm per metre — without it, the boards will buckle and damage the underlay. Fasteners are driven at a distance of at least 10 mm from the edge of the board, otherwise the edge breaks under wind load. In valleys and around dormer windows, the base is made from a single piece of plywood or OSB without joints — a joint in these areas causes a crack in the waterproofing within a year or two. The seams between boards must be located over the counter-battens: if a seam falls between the battens, the base will be weak at that point and may break through, so before installation it is checked that every joint is supported by a batten.
The role of the underlayment and valley carpet
The base for soft roofing is a common question, so let us examine it in detail. Underlay and valley lining are additional waterproofing in the most vulnerable areas of the roof. Let us look at where they are mandatory and how to install them correctly.
Underlayment — continuous or partial
The underlay is laid on the continuous base and can be continuous (over the entire area) or partial (only in valleys, on eaves and the ridge) — the choice depends on the roof slope. On slopes with an inclination of 12–20°, a continuous underlay is mandatory over the entire base; on steep roofs (from 20°), partial laying is sufficient: a strip of 500 mm along the eaves, 250 mm on each side of the valley, 150 mm on the ridge and around pipes. The material is unrolled in horizontal strips from bottom to top with an overlap of 100–150 mm, fixed with roofing nails at a spacing of 200 mm and the joints are sealed with bituminous mastic or self-adhesive tape. On complex configurations with many abutments, a continuous underlay adds 15–20% to the budget, but eliminates the risk of leaks in snow accumulation zones — on attic roofs with slopes of 15–18°, saving on partial laying results in warranty repairs after two seasons. With a slope of less than 20°, an underlay is mandatory over the entire area — this is a requirement of all flexible shingle manufacturers, and violating it voids the warranty.
Valley lining — reinforced waterproofing in the valleys
The valley carpet is a reinforced waterproofing material that is laid in the valleys over the underlayment and protects the most complex roof unit from leaks. It differs from the underlayment in its greater thickness (3–4 mm versus 1–2 mm) and the presence of a bitumen layer on both sides — this allows it to withstand the hydrostatic pressure of water flowing from two slopes at once. The carpet is rolled out along the valley axis, the roll width is usually 1000 mm, but in areas with intense precipitation in the foothills (Butakovka, Kok-Tobe) we recommend laying two layers with a total overlap of up to 1500 mm. Each edge is fixed with nails every 150–200 mm and coated with bitumen mastic to a width of 50 mm. The valley carpet cannot be replaced with ordinary underlayment, even in two layers — because of its one-sided bitumen coating the latter does not withstand hydrostatic pressure and leaks within a year or two, which is especially critical on roofs with a slope length of more than 8 m.
How to make a valley on a soft roof correctly
The valley is made as follows: an underlayment is laid on the continuous deck, on top of it a valley carpet 500–1000 mm wide (250–500 mm on each slope), then shingles with trimming along the valley axis. The trimming technique is critical: the shingles are brought onto the valley by 150–200 mm, after which each row is cut at an angle of 45–60° to the valley axis, forming an open channel 100–150 mm wide. Bitumen mastic is applied to the back of each shingle in the area where it meets the valley carpet, and additional fixing is done with nails at a distance of 150 mm from the cut line so as not to damage the waterproofing. In projects with sharp temperature swings (from –30° in winter to +40° in summer), trimming with a gap of 120 mm works more reliably than the minimum 100 mm — on one site in the suburbs, after a winter with frequent thaws, a gap of 90 mm produced capillary suction 40 cm high along the rafters. The shingles in the valley should not reach the valley axis by 100–150 mm — this creates an open channel for water, otherwise capillary suction forms at the joint.
Pipe and ventilation shaft penetration details
To seal pipe and ventilation shaft penetrations, special penetration elements (sleeves, aprons) and bitumen mastic are used — the junction point must be raised above the roof level by 200–300 mm. The process is as follows: a hole is cut around the pipe in the continuous deck with a gap of 10–15 mm, then a rubber mushroom sleeve is placed over the pipe, its lower flange glued to the underlayment with bitumen mastic and additionally fixed with nails in a circle. On top the sleeve is covered with shingles, which are cut to the shape of the pipe and coated with mastic to a width of 50–70 mm. For rectangular shafts a metal apron with a 200–300 mm fold onto the walls is made — it is installed before laying the shingles, and the top edge is set into a groove in the wall and sealed with silicone sealant. Around pipes and shafts an additional layer of underlayment is always made with a turn-up onto the vertical surface — without this a capillary gap forms at the junction, which expands in winter when condensation freezes.
Ridge and eaves — how to finish the junctions
The ridge is finished with ridge-and-eaves shingles, which are cut into individual elements and installed with a 50–70 mm overlap, while the eaves are protected with a metal eaves strip and a drip edge. The order of work: first the drip edge (a metal strip with a drip deflector) is fixed to the eaves board, then on top of it the eaves strip, which covers the edge of the continuous deck and the underlayment. The shingles at the eaves are hung 10–20 mm over the edge of the strip so that water flows directly into the gutter. At the ridge between the slopes a 50 mm ventilation gap is left, into which a ridge aerator is installed — a plastic profile with perforation, hidden by the ridge-and-eaves shingles. Each element of the aerator is fixed to the base with nails at a pitch of 200 mm, and the joints between sections are glued with bitumen tape. A ridge aerator must always be installed at the ridge — without it the ventilation of the under-roof space does not work, and moisture accumulates under the shingles, causing the rafters to rot after just 3–5 years of use.
Ventilation of the under-roof space
Ventilation under soft roofing is not an option but a mandatory condition for the durability of the rafter system and insulation. Let us look at how to organise air circulation, what elements are needed and what their absence leads to.
What ventilation gap is needed under a soft roof
The ventilation gap under soft roofing must be at least 50 mm — this is the distance between the diffusion membrane and the continuous OSB deck, created by a counter-batten made of 50×50 mm timber. On short slopes up to 6 metres this is sufficient, but on long slopes of 10 metres or more specialists recommend increasing the gap to 60-70 mm, especially in Almaty's conditions with sharp temperature swings and high humidity in spring. With a gap of 30-40 mm the airflow rate drops so much that moisture cannot be removed in time — condensation remains on the rafters and the underside of the OSB, and after 2-3 seasons the wooden elements begin to rot. Reducing the gap to 30-40 mm lowers ventilation efficiency by 30-40% — the air cannot remove moisture in time, so during installation check the height of the counter-batten with a tape measure, as some crews cut corners and use 40×40 mm timber.
How to ventilate under a soft roof — diagram and components
Ventilation under soft roofing works on the principle: air enters through the eaves soffit with 10-20 mm vents, rises through the 50 mm ventilation gap and exits through a ridge aerator or point aerators on the slopes. For intake, perforated soffits or eaves strips with ventilation mesh are used — in Almaty cottage communities (Gorny Gigant, Kargaly) they are often replaced with ordinary board sheathing with gaps, which reduces intake by 40-50% and makes the ventilation gap useless. The exhaust is installed at the highest point: a ridge aerator is cut into the ridge line along its entire length, and point aerators (one per 60-100 m² of roof) are installed on the slope closer to the ridge. The area of ventilation openings should be 1/300 of the roof area — if made smaller, ventilation cannot cope with the volume of moist air, and condensation will appear even with the correct gap.
Ridge aerator and point aerators — which to choose
| Parameter | Ridge aerator | Point aerators |
|---|---|---|
| Location | Along the entire length of the ridge | On the slopes, 1 pcs per 60-100 m² |
| Efficiency | High (even extraction) | Average (depends on the quantity) |
| Suitable for | Gable and mono-pitch roofs | Hipped, pyramidal and complex roofs |
| Installation | Simple (cut at the ridge) | More complex (requires a roof penetration) |
| Aesthetics | Invisible on the ridge | Visible on the slope |
Both types can be combined on a single roof: a ridge aerator for the main volume and point vents for areas where there is no ridge — for example, on hip roofs of country houses in Almaty.
What happens if ventilation is not provided
Without ventilation beneath soft roofing, condensation accumulates on the waterproofing and rafters, leading to wood rot, wetting of the insulation and destruction of the OSB base within 3-5 years. Warm moist air from the living spaces rises to the roof, meets the cold membrane and turns into water droplets — with a gap of less than 50 mm they do not have time to dry out and are absorbed into the timber. In Almaty houses with attics this problem is aggravated by frequent winter thaws: during the day the snow melts on the roof, at night it freezes, and the freeze-thaw cycles destroy the OSB structure within 2-3 seasons. The first sign of missing ventilation is mould on the rafters on the attic side and swelling of the shingles on the roof in summer due to overheating, so if these symptoms appear, aerators must be installed immediately, without waiting for a major overhaul.
Errors in the installation of soft roofing
Even quality materials will not help if mistakes are made during installation. Let us look at the most common problems and how to avoid them.
Mistake 1 — wrong base (cutting costs on OSB/plywood)
The most common mistake is using OSB-2 instead of OSB-3 or FK plywood instead of FSF, as well as boards that are too thin (6 mm instead of 9-12 mm), which leads to deflection of the base and damage to the shingles. OSB-3 differs from OSB-2 in its increased moisture resistance: with temperature fluctuations in the attic, condensation does not destroy the board. FSF plywood, unlike FK, is bonded with phenol-formaldehyde glue that is resistant to delamination in a damp environment. The thickness is selected according to the rafter spacing: with a spacing of 600 mm, 9 mm OSB-3 is sufficient; with a spacing of 900 mm — 12 mm. In the local climate with frequent thaws and snowfalls, it is especially important not to economise on the moisture resistance class. Saving 200-300 KZT on a sheet of OSB results in replacing the entire roof after 3-5 years — the base simply rots from condensation.
Error 2 — missing or incorrect vapour barrier
The second most common mistake is the absence of a vapour barrier or laying it on the wrong side, which causes the insulation to get wet, lose its thermal insulation properties and begin to rot. Most vapour barrier films have two sides: smooth (polypropylene) and rough (with an anti-condensation coating). The rough side always faces into the room so that condensation droplets are retained on the fibres and evaporate back into the room. The smooth side prevents moisture from penetrating into the insulation. If the sides are mixed up, vapour from the house passes freely through the film and settles in the mineral wool — the thermal conductivity of the insulation increases 2-3 times. On Almaty projects with 200 mm stone wool this means heat loss of up to 40% in winter. If the vapour barrier is laid with the smooth side towards the insulation, condensation accumulates inside the build-up — this can be noticed by damp patches on the ceiling of the upper floor.
Error 3 — poor ventilation (no counter-battens)
The third common mistake is installing OSB directly on the waterproofing without counter-battens, which blocks ventilation and leads to rotting of the rafters and insulation due to condensation accumulation. Without counter-battens, the waterproofing membrane lies tightly against the base — moisture that has seeped through the shingle joints or condensation from the underside of the OSB does not evaporate. As a result, within 2-3 seasons, mould forms under the roof and the rafters lose their load-bearing capacity. The counter-battens create a gap of 30-50 mm between the waterproofing and the base — this is the only way to ensure air circulation and remove moisture from the roof assembly.
Conclusion
A properly designed soft shingle roof is an engineering system where every layer affects the durability of the whole house. We have covered the main principles worth remembering.
Key takeaways
- The base is the foundation of the roof: a continuous base of OSB-3 or FSF plywood 9-12 mm thick is a mandatory condition for the durability of soft shingles. Saving on thickness or grade of board leads to deformation of the covering.
- Ventilation is the key to a dry roof build-up: a counter-batten 30-50 mm high and vents in the eaves and ridge ensure air circulation. Without them the insulation gets wet, and the rafters begin to rot after 3-5 years.
- Every unit requires attention: the valley, junctions to pipes and walls are the most vulnerable points. Using a valley carpet and correctly sealing these areas prevents leaks.
- Mistakes made at the installation stage cannot be corrected without dismantling: incorrect vapour barrier, absence of counter-battens or a weak base are problems that cannot be resolved without completely redoing the roof.
- Design and calculation are the key to success: accurate calculation of the quantity of materials, roof pitch angle and shingle layout pattern by 30% reduces the risk of installation errors.