Tank welding: vertical cylindrical tank fabrication technology from bottom to roof

Reading time: 18 minutes
Tank welding — a welder in a protective mask welding a seam of a large steel tank at an industrial site

Tank welding is a set of technological operations for the assembly and welding of vertical steel tanks (VST) for storing petroleum products, water and flammable liquids. It includes the roll and sheet-by-sheet erection methods, automatic, semi-automatic and manual arc welding, mandatory quality control and hydraulic testing.

Tank types and their design — from RVS to RGS

Types of VST and HST tanks — vertical and horizontal steel tanks at a petroleum depot

Tank welding begins with an understanding of the structure: the main object is a vertical steel tank (RVS). Let us look at what types there are, what elements they consist of and how the structures differ for different media.

What an RVS is and what elements it consists of

An RVS (vertical steel tank) consists of a bottom (panel plus annular plates), a shell of 4–12 courses, a roof (fixed or floating) and process nozzles. The bottom is assembled from a central panel and annular edge plates around the perimeter — the edge plates take the load from the shell and transfer it to the foundation. The shell is built up from courses: each course is a ring of welded plates with a thickness of 6–25 mm depending on the volume and height of the tank. The roof may be conical (panel), spherical (frameless) or floating (pontoon). The number of shell courses depends on the volume: for RVS-5000 — 6–8 courses, for RVS-20000 — up to 12. Process nozzles (inlet, outlet, manholes) are welded into the lower shell courses. If the tank on site is assembled by the sheet-by-sheet method, each course is erected and welded sequentially from the bottom up — this sequence minimises shell deformation during welding.

Tank types — fixed roof, floating roof, pontoon, RGS

RVS tanks with a fixed roof are used for water and low-viscosity oil products, while those with a floating roof (pontoon) are used for petrol and flammable liquids to reduce evaporation losses. RGS (horizontal tanks) are used for small volumes — up to 200 m³, and are installed at filling stations and in boiler houses. The floating roof moves along guides inside the tank, rising and falling with the liquid level — this eliminates the gas space above the product. In a pontoon tank the fixed roof remains, and the pontoon (floating disc) sits on the liquid surface beneath the roof. For tanks holding oil products and flammable liquids, the requirements for seam tightness and welder certification are stricter — all critical seams are made by specialists with NAKS approval in accordance with the design. At facilities in the Karaganda region, pontoons are always specified for petrol depots, even if the design permits a fixed roof — the difference in evaporation losses over a year pays for the installation of the pontoon within 2–3 seasons.

Comparison of tank types by design and application

Tank typeDesignVolumeApplicationWelding specifics
Vertical cylindrical tank with a fixed roofBottom + wall + conical/spherical roof100–50000 m³Water, fuel oil, diesel fuelAll welds under control, hydrotesting
Vertical cylindrical tank with a floating roof (pontoon)Bottom + wall + pontoon on the liquid surface1000–100000 m³Petrol, flammable liquids, oilIncreased requirements for wall tightness
Horizontal cylindrical tankCylindrical shell on supports5–200 m³Fuel, oils, water at filling stationsWelding longitudinal and circumferential seams

For flammable liquids a floating roof or pontoon is mandatory — this is an industrial safety requirement, not merely a recommendation: without a pontoon the concentration of petrol vapour under a fixed roof reaches explosive values at temperatures above +25 °C.

Tank assembly methods — rolled and sheet-by-sheet

Tank assembly methods — roll and sheet-by-sheet methods of installing steel sheets on the construction site

Tank erection begins with the choice of assembly method — rolled or sheet-by-sheet. Let us look at how they differ, what advantages each has and which projects each suits.

Roll assembly method — how the wall is rolled into a coil

With the rolled method, a shell panel up to 18 m long is welded at the factory or on a jig, rolled into a coil and delivered to the site, where it is unrolled and installed on the bottom. At Kazakhstan oil depots in the Atyrau and Mangystau regions, coils weighing up to 30 tonnes are unrolled with KS-55730 cranes or tracked DEK-631 — cranes; the single erection seam of the unrolled panel is made by automatic submerged arc welding (ADF-1002, ADF-1250) with edges prepared to an X-shaped profile. The bottom is assembled from rolled panels, and the roof — from panel elements or also rolled into a coil. A minimum of seams remains on site: the vertical seam on the shell, the bottom joints and the roof junction assemblies. The rolled method reduces erection time by a factor of 2–3 compared with the sheet-by-sheet method, but requires a crane with a lifting capacity of 30 to 50 tonnes — if there is no heavy equipment on site, the coil cannot be unrolled and it will have to be cut into parts, losing all the advantages of the method.

Sheet-by-sheet assembly method — installation from individual course sheets

The sheet-by-sheet method — each shell course is assembled from 4–8 individual plates, which are welded with vertical seams on site. The method is used on tanks with a volume from 20000 m³ and where crane access is limited: in the cramped conditions of Almaty's industrial zones (the territory of CHPP-2, the BAD industrial zone) a crane with a lifting capacity of up to 10 tonnes delivers plates weighing 1,5–3 tonnes, and the erectors align them by plumb line and clamps. Each subsequent course rests on the previous one, so the geometry is checked at every tier — deviations from the vertical, ovality and edge misalignment are measured. Vertical seams are welded semi-automatically (Lincoln Electric Power Wave 455M, Kemppi FastMig X) with flux-cored wire or by manual arc welding with UONI-13/55 electrodes, and horizontal seams — by submerged arc or the same semi-automatic method. With the sheet-by-sheet method it is easier to correct the geometry of each course before welding the next one — vertical deviations are corrected on site, not after the entire panel has been rolled out.

Comparison of the coil and sheet-by-sheet methods — which to choose

ParameterRoll methodSheet-by-sheet method
Tank volumeUp to 10000–20000 m³From 5000 m³, optimal from 20000 m³
Number of installation jointsMinimum — only the vertical seam of the unrolled shellMaximum — every sheet is welded on site
Wall installation time2–5 days10–30 days
Crane requirementsLoad capacity 30–50 t for the coilUp to 10 t for individual sheets
Geometry controlHarder to correct after rotationEach course is inspected separately
Typical applicationTypical RVS tanks at oil depots, for waterLarge tanks, confined conditions

Tank welding methods — automatic, semi-automatic, manual

Tank welding methods — automatic submerged arc welding and manual arc welding on the tank shell

Three main methods are used in tank fabrication: automatic submerged arc, semi-automatic in shielding gases and manual arc. Each has its own field of application and limitations regarding seam position.

Automatic submerged arc welding (SAW) — for circumferential seams of the bottom and wall

Automatic submerged arc welding (SAW) is used for the circumferential seams of the bottom (the joint between the sheet and the edge plates) and the horizontal seams of the shell — this is the most productive method, delivering consistent seam quality. A welding tractor (submerged arc machine) moves along a rail track or magnetic strip, feeding the electrode wire under a layer of granular flux — the arc burns inside the flux cushion, fully isolated from the air, which eliminates spatter and metal oxidation. On tanks made of 09G2S and 16GS steel with a thickness of 10–20 mm, the speed reaches 25–30 m/h at a current of 500–800 A, and a single pass forms a seam with a penetration depth of up to 12 mm. On low-alloy steels, ceramic flux is used — it provides optimal mechanical properties of the weld metal and fewer pores compared with fused flux.

Semi-automatic welding (MIG/MAG/FCAW) — for vertical wall welds

Semi-automatic welding in CO₂ or an Ar+CO₂ mixture (MIG/MAG) is used for the vertical shell seams and erection joints — the method provides a speed of 8–15 m/h and good seam formation in the vertical position thanks to controlled droplet transfer. The welder moves the torch upwards along the groove while the feeder pushes continuous wire (Sv-08G2S, 1,2–1,6 mm diameter) or a flux-cored strip (FCAW) — the latter gives a more stable arc in wind and draughts on an open site. Shielding gas is supplied through the torch nozzle at a flow rate of 12–18 l/min; on the erection joints of the shell of an RVS 5000 m³, 70–80 vertical passes of 2–2,5 m each are made semi-automatically. At temperatures below -10°C the process is carried out with preheating of the edges to 100–150°C — this is a mandatory requirement to prevent cracks in the heat-affected zone.

Manual metal arc welding (MMA) — for tack welds, nozzles and repairs

Manual arc welding (MMA) is used for tack welds during assembly, welding of nozzles, branch connections and repair work — for critical tank seams, electrodes of the UONI-13/55 (E50A) or LB-52U type with a diameter of 3–4 mm are used. The process is carried out on direct current with reverse polarity at a current of 120–180 A, the speed does not exceed 2–5 m/h, and the penetration depth per pass is 3–5 mm — this is 3–4 times slower than the automatic method, so only short seams and areas inaccessible to mechanised equipment are welded manually. Tack welds on the bottom 50–80 mm long are placed every 300–400 mm along the contour of the panel, and Du100–300 nozzles are welded with argon purging from the inside to prevent scale. Manual welding gives the greatest control in hard-to-reach places — the corner weld, branch connection zones — but its share in the total seam volume of a modern tank does not exceed 10–15%.

Comparison of welding methods — where to use each

Welding methodType of seamsProductivityWeld qualityEquipment
Automatic submerged arc welding (SAW)Circumferential joints of the bottom and wallHigh (up to 30 m/h)Stable, minimal defectsWelding tractor + flux
Semi-automatic (MIG/MAG/FCAW)Vertical wall seams, assembly seamsAverage (8–15 m/h)Good with the correct modeSemi-automatic + wire + gas
Manual metal arc (MMA)Tack welds, nozzles, repairsLow (2–5 m/h)Depends on the welder's skillInverter + electrodes

On large tanks (from 10000 m³) up to 70% of the seam volume is done by automatic welding, 25% — by semi-automatic and only 5% — manually.

Tank welding technology — the order of assembling the bottom, wall and roof

Tank welding technology — sequential assembly and welding of the bottom, shell and roof of a steel tank

The tank assembly technology follows a strict sequence: first the bottom, then the shell course by course, then the roof. Violating the order leads to deformation and defects.

Welding the tank bottom — from the sheet panels to the annular plates

Assembly of the bottom begins with the panel — the central plates are butt-joined by automatic submerged arc welding, then the edge plates (peripheral plates) are welded with an overlap or butt joint to the panel. The long seams of the central panel are welded from the middle to the edges to compensate for metal shrinkage. The bottom edge plates are 2–4 mm thicker than the central panel — they take the load from the shell and the corner weld. At Almaty tank farms there are bottoms made of 09G2S steel 6–12 mm thick, where the edge plates reach 14–16 mm. Welding of the edge plates is carried out with mandatory vacuum box testing — brushing with soap solution reveals the slightest pores that might go unnoticed on the central panel.

Welding sequence for the wall courses — from the first to the last

The shell courses are welded sequentially from the bottom up: first the bottom course is welded to the bottom plate, then the second, third and so on up to the top. Each course is first assembled with tack welds, then the vertical seams are welded, followed by the circumferential ones — this sequence prevents the seam from “pulling” the shell geometry. Here automatic submerged arc welding of tanks forms the vertical joints of each course on a flux backing, ensuring root penetration without back-gouging. The circumferential seams between courses are welded semi-automatically in CO₂ — this method gives high productivity when welding in the flat position. The sequence of assembling the courses — from the bottom to the top — is not accidental: each overlying course fixes the geometry of the one below, preventing the shell from “drifting” vertically.

Welding the corner joint — joining the bottom and the wall

The bottom corner joint — the annular plate-to-shell weld — is the most critical assembly in a tank, connecting the bottom to the first course of the shell. It is welded with a fillet weld with mandatory reinforcement, often in two passes: first semi-automatically, then by manual back-welding. The fillet weld leg of the bottom corner joint for RVS-2000 is 8–10 mm, and for RVS-5000 it reaches 12–14 mm depending on the thickness of the shell and bottom. After welding, the bottom corner joint must be checked by visual and measuring inspection (VMI) and ultrasonic testing (UT) — this is the only way to detect lack of fusion at the weld root. The bottom corner joint experiences the maximum stresses from the hydrostatic pressure of the product, so its inspection is a mandatory stage: visual, UT and hydrostatic testing.

Welding the roof — fixed and floating

A fixed roof (conical or spherical) is assembled from petal-shaped sectors, welded with radial and circumferential seams. Radial seams are welded from the centre to the periphery to avoid sagging of the sheets between the trusses — especially critical for conical roofs with a span of more than 12 metres. A floating roof (pontoon) is welded from sealed box compartments, each of which is tested for tightness with soap solution under a pressure of 0,05–0,1 MPa. For a floating roof, the tightness of each compartment is critical — product entering the pontoon leads to loss of buoyancy and jamming of the roof.

Welding the tank wall and controlling deformation

Shell welding is the most extensive stage: up to 70% of the total seam length falls on the vertical and horizontal joints of the courses. Here the technique for making vertical seams and the methods of preventing deformation are critical.

Technique for vertical wall seams — top-down or bottom-up

The vertical seams of the tank shell are welded using the downward method (top to bottom) — the speed reaches 15 m/h, and seam formation is more stable thanks to the smaller volume of deposited metal. Semiautomatic welding with 1,2 mm wire in CO₂ shielding produces a 6–8 mm leg in a single pass without repositioning; with a sheet thickness of up to 12 mm, the weld pool moves downward under gravity and does not flow into the gap, preventing undercuts. The upward method (bottom to top) is used less often — for thick-walled tanks (shell thicker than 20 mm) or the root pass, where greater penetration and a controlled backing bead are needed. At Kazakhstani sites, the shell thickness of RVS tanks rarely exceeds 16 mm, so downward technique is the main standard for vertical seams: on RVS-5000 with a height of 12 m, the vertical joints of all eight courses are welded top to bottom without switching to the upward method.

Backstep method — how to prevent deformation

The back-step method is welding a long seam in sections of 200–400 mm in the direction opposite to the overall direction: each subsequent section overlaps the previous one by 20–30 mm, evenly distributing heat input along the length of the joint. For the circumferential seams of the bottom and shell, this method reduces residual deformation by 30–50% compared with welding “straight through” (from the centre to the edge without splitting into sections). In practice, a circumferential seam 18 m in diameter is divided into 12–16 sections and welded in a staggered sequence: the first section is welded, two are skipped, then the skipped one is returned to — each section has time to cool to 100–150°C, which minimises plate warping. The method is especially effective for the first shell course: deformation at this height is critical for the geometry of the entire tank, and the back-step technique keeps vertical deviations within 5–8 mm instead of 15–20 mm with continuous welding.

Typical tank seam defects — causes and prevention

DefectCauseHow to preventDetection method
PorosityFlux/gas moisture, draught, oil contamination of the edgesFlux calcination at 300–350°C, wind protection, cleaning down to bare metalVIK, ULTRASONIC TESTING
Lack of fusionLow current, excessive speed, narrow gapMode according to the welding chart (180–220 A for 1,2 mm wire), gap 2–4 mmUT, radiography
CracksHigh joint stiffness, temperature below –10°CEdge preheating to 100–150°C, backstep methodVIK, radiography
UndercutsExcessive current, electrode angle more than 20° from verticalCurrent reduction of 10–15%, angle no more than 15° from the normalVIK (welder's template)
Wall deformationsUneven heat input when welding the coursesBackstep method, clamping with G-clamps every 1,5–2 mVIK, levelling

More than 60% defects are detected by visual inspection — they are fixed before UT or radiography, saving 2–3 shifts on RVS-5000.

How to avoid wall deformation when welding the courses

The main deformations of the shell are “bulges” (local buckles of up to 10–15 mm) and vertical deviations (courses leaning inwards or outwards). They are prevented by securing the courses with clamps and braces at 1,5–2 m intervals around the perimeter, and the welding sequence is set from the centre of the course to the edges — the metal expands without forming folds. When welding vertical seams on the second and third courses, overheating of a single section is avoided by pausing for 3–5 minutes between passes so that the thermal field evens out. GOST 31385-2016 regulates the permissible deviations: for a tank 12 m high — no more than 30 mm over the entire height, local bulges — no more than 1,5% of the shell radius. Exceeding these tolerances is grounds for cutting out and rewelding the defective course, which adds 2–3 days of work; therefore during erection of RVS-5000 the geometry is checked after each course, not once the shell assembly is complete.

Quality control of welded joints and tank testing

The quality of the tank's seams is inspected at every stage — from visual examination to hydrostatic testing. Let us go through all the inspection methods and safety requirements.

Visual and measuring inspection (VMI) — the first stage of inspection

Visual and dimensional inspection (VDI) is carried out after each welding pass — the seam geometry and the absence of undercuts, pores, cracks and overlaps are checked. All seams are examined with the naked eye and with a 4–10× magnifier. UShS templates (universal welder's gauge) and a vernier calliper allow the width, reinforcement height and leg of a fillet weld to be measured — deviations of more than ±1 mm from the design are recorded as a defect. During the installation of RVS-5000 in Aktau, PROFI-DOM specialists identified 12 metres of unacceptable undercuts on the first course of the shell precisely by VDI, which prevented hidden metal loss 2–3 mm deep. VDI is mandatory for 100% of the tank's seams — without a positive conclusion, no transition is made to the next inspection methods (UT, radiography).

Bottom tightness testing — vacuum box and kerosene-chalk test

The tightness of the bottom seams is checked with a vacuum box — a soap solution is applied to the seam, and a box with a vacuum of 0,06–0,08 MPa is placed on top; the appearance of bubbles indicates a defect. For inaccessible areas, the kerosene-chalk test is used: the seam is wetted with kerosene on one side and with a chalk solution on the other; after 30–60 minutes, the kerosene reveals through cracks as dark spots. The vacuum box detects not only through defects but also surface defects from 0,5 mm deep, which is critical for tanks containing flammable liquids — a microcrack in the chime seam of the bottom turns into a rupture up to 200 mm long during hydrostatic testing. In PROFI-DOM's practice, on RVS-2000 for diesel fuel, 4 hidden pinholes were recorded at the joint between the edge plate and the central part of the bottom using the vacuum box — the kerosene test did not reveal them.

Non-destructive testing of welds — UT and radiography

Ultrasonic testing (UT) and radiographic testing (X-ray) are used to detect internal seam defects — cracks, lack of fusion and slag inclusions. The scope of testing is specified by the design: for vertical shell seams of the tank — 100% UT or radiography, for horizontal ones — at least 25% of the length of each seam. UT is more effective than radiography on metal thicknesses up to 30 mm — it detects planar defects (cracks, lack of fusion) with an opening from 0,1 mm, whereas X-ray misses them when oriented parallel to the beam. On the shell of VST-10000 in Shymkent we performed 48 metres of UT per shift versus 14 metres of radiography — the 3,4-fold difference in speed reduced crew downtime. UT is preferable to radiography for tanks at operating sites — it is safer and faster, but requires a highly qualified operator.

Hydraulic testing of the tank — final strength check

Hydrostatic tests are carried out after all work is completed — the tank is filled with water to 100% of its design volume and held under pressure exceeding the working pressure by 25% for 10–30 minutes. During the process, the absence of leaks, deformations and pressure drop is monitored. For RVS-3000 with a height of 12 metres, the test pressure is 0,15 MPa against a working pressure of 0,12 MPa — the difference of 25% makes it possible to detect hidden defects in the installation seams that do not appear at working pressure. At one site in Atyrau, during the hydrostatic testing of RVS-5000, we discovered local bulging of the bottom edge plate by 8 mm — the cause turned out to be lack of penetration in the chime seam, which had not been detected by UT due to the complex geometry. Hydrostatic testing is mandatory for all new RVS tanks — it confirms that the structure will withstand the design loads in service.

Safety requirements for welding and repairing tanks

Work on tanks containing flammable liquids is carried out only after degassing (steaming, washing, ventilation) and the issue of a hot work permit. Steaming is performed with live steam at 100–110 °C for 6–12 hours depending on the tank volume, after which an air sample is taken with a gas analyser — the content of oil product vapour must not exceed 0,1% of the lower explosive limit. Welders must hold NAKS certification for the relevant type of work (H1 — tanks and gas holders) and an electrical safety group of at least II. Welding of non-degassed tanks is strictly prohibited — even a spark from the welding arc can cause an explosion of fuel vapour — there have been cases at oil depots when attempts were made to weld up a leak without steaming.

Conclusion

Tank welding is a multi-stage process with dozens of engineering solutions; the final quality determines the tightness and safety of the facility for decades.

Key takeaways

  • Assembly technology — VST tanks are erected by the roll or sheet-by-sheet method; the choice depends on the metal thickness and site conditions, and the roll technology reduces the volume of erection seams by 30–40 %.
  • Joining methods — automatic submerged arc (bottom and horizontal shell seams), semi-automatic (vertical shell seams and erection joints), manual (tack welds, nozzles and repairs); the automatic method provides stable penetration without defects over a course length of up to 18 metres.
  • Quality control — every seam undergoes visual, instrumental and non-destructive testing (UT, radiography, vacuum box); final hydrostatic tests confirm strength and rule out hidden leaks.
  • Safety — welding and repair of tanks containing flammable liquids are carried out only after degassing and under a work permit; welders must hold NAKS certification, otherwise the QC report will not be signed.
  • Deformations — the backstep welding method and the correct sequence of seam deposition minimise warping of the shell and bottom, and without this technique the gap in the joint may exceed the tolerance of 2 mm per metre.

About the author

Kanat Serikov

Welding engineer for tank structures (NAKS certification); works with the PROFI-DOM workshop. Explains the methods and technology of tank welding: roll and sheet-by-sheet assembly, bottom, shell, tightness inspection.

More than 16 years in the installation and welding of RVS tanks; automatic submerged arc welding, semiautomatic welding, seam inspection with a vacuum box and X-ray, and hydrostatic testing of tanks.

Frequently asked questions
What tank welding methods are used in Almaty?
They use roll and sheet-by-sheet assembly, as well as automatic, semiautomatic and manual arc welding.
How much does welding a vertical cylindrical tank cost in Kazakhstan?
The price depends on the scope, metal thickness and complexity of the work. The exact cost is calculated after a specialist visits the site.
Which tanks are welded more often — VST or HST?
In Almaty and the region, vertical tanks (RVS) are most often ordered for storing petroleum products and water.
Are hydraulic tests required after welding?
Yes, they are mandatory. They confirm the tightness and strength of the seams before the tank is put into operation.
How is the quality of tank welded joints controlled?
Non-destructive testing is used: ultrasonic, X-ray and dye penetrant inspection.
Can the tank be welded on site in Almaty?
Yes, the sheet-by-sheet method allows the tank to be assembled directly at the customer's site.
What documents are needed for tank welding in Kazakhstan?
A design, material certificates and concealed work reports are required. All stages are coordinated with technical supervision.